wetgrind-1

Why wet grind?

In this technical paper, we explore the effects of wet grinding versus dry grinding on Tungsten electrodes used in TIG welding. Through a preliminary experiment, we examine the post-welding condition of Tungsten electrodes ground using both methods after a 10-minute TIG welding session.

Category: Artigos

Benefits of wet grinding

  • The liquid for cooling prevents the electrode from overheating and results in a polished and even surface of the Tungsten electrode.
  • The liquid serves as a barrier against dust generated during the grinding process. By effectively suppressing dust emissions, wet grinding reduces the risk of inhalation and exposure to hazardous particles, promoting a safer working environment for welders.
  • Enhances the durability and longevity by hindering destruction of the electrode caused by the halo effect.
  • Ensures consistent performance during welding operations by maintaining a similar penetration level of the weld pool.

 

Halo effect

The Halo effect occurs during TIG welding further up on the tip of the electrode, which creates a beard-like protrusion, as shown in the second photo above under ”Dry grinding”.

This beard-like protrusion damages the electrode, which negatively affects the weld quality, particularly noticeable in the penetration of the weld pool, which is indicated on the next page.

Dry-ground electrodes show faster degradation compared to wet-ground electrodes, which is demonstrated above.

This highlights the importance of wet grinding to prolong the longevity of the electrode tip and ensure better welding results.

Safety

Safety is a key factor when grinding Tungsten electrodes.

The Ultima-TIG wet grinder’s enclosed chamber reduces the risk of accidents compared to open bench grinders. Its dust collection system prevents harmful Tungsten particles from being inhaled, protecting the user’s health. Proper disposal of the collected dust further reduces exposure risks. The secure design also prevents direct contact with the grinding disc, eliminating the chance of burns or cuts. Additionally, the electrode holder ensures safe handling and reduces the danger of overheated electrodes, making the Ultima-TIG a safer choice for welders.

Welding conditions

Electrodes ground at 30°

5 welds of 150 seconds each

All welds are effectuated at 200 Amps

Weldingspeed: 89 mm/min

Base material: Stainless steel AISI 304.
Download

Dry grinding

Mais conteúdo

truncate technical paper

Benefits of a truncated electrode tip

16. Junho, 2026
In TIG welding, several factors influence the quality and shape of the arc In addition to material, power source, current... Saiba mais

Entre em contato connosco

Tem qualquer pergunta sobre os nossos produtos ou outro assunto? Sinta-se à vontade para entrar em contato connosco através do formulário de contato, uma mensagem e-mail ou telefone diretamente para nós. Será um prazer entrar em contato consigo.

Inelco Grinders Logo

Contato

Não perca algo importante

Assine a nossa newsletter e receba diretamente as mais recentes novidades da Inelco Grinders®.

Marque uma demonstração gratuita

Os nossos afiadores de tungsténio diminuem de até 50% o desgaste dos elétrodos de tungsténio. Está interessado em avaliar quando poderá economizar e como os nossos afiadores podem atender às suas exigências de soldadura? Insira os seus dados logo abaixo e asseguramos que o nosso distribuidor mais próximo entrará em contato consigo para encontrarem a solução mais apropriada para si.

  • Este campo está escondido ao visualizar o formulário
  • Este campo está escondido ao visualizar o formulário
  • Este campo está escondido ao visualizar o formulário

Get in touch with a distributor

Please fill out the form – and we will connect you with a distributor in the USA.